塑料成型
2. Peeling/Delamination
Fig.2.1:Peeling and delaminationcaused by strange material in thegranules
Position 1
Position 2
Fig.2.2:Partial cross section through Fig.2.1:(sample thickness 1.5 mm)
Fig.2.3:Position 1
Fig.2.4:Position 2
3. Weld line
Fig.3.1:Weld line notch; vertical illumination,
magnification 11:1
Fig.3.3:Weld line (metallic effectcoloring)
Fig.3.2:Weld line notch; transmitted light,polished,magnification 560:1
Fig.3.4:Color marking in theweld line; vertical illumination,dark field,magnification 52:1