5. Sink marks
(front elevation and section)
Fig.5.1:Sink markon the visible side(Cause:Materialaccumulation asshown in Fig.5.2)
Fig.5.2:Materialaccumulation(avoidable by suitable recessing)
6. Voids
Fig.6.1:
Voids at the end of the flow path in a cup
13